| 0-5MM crushed sand |
| 5-12 MM aggregate |
| 12-22 MM aggregate |
| 12-38 MM aggregate |
| TEST NAME | STANDARD | VALUE OF STANDARD | VALUE OF NORDEKA |
| Resistance to Degradation ( LA) | TS EN 1097-1 | Max. %35 | 27 - 28,5 % |
| Soundness Mg2S04 | TS EN 1367-2 | Max. %15 | 1% |
| Soundness Na2S04 | TS EN 1367-2 | Max. %18 | 1,5% |
| Flatness Index | TS EN 933-3 | Max. %15 | 7-8 % |
| Specific Weight gr/cm3 | TS EN 1097-6 | Min. 2,60 | 2,72 |
| Org.Material determination | TS EN 1744-1 | Max. %2 | 0% |
| Water Absorption | TS EN 1097-6 | Max .%3 | 0,20% |
| Methylene Blue | TS EN 933-9 | Max .%1,5 | 0,50% |